Re: 28-30-120 learning curve
Reply #15 - Oct 12th, 2016 at 12:37am
Print Post  
Travelor,

Rocky Mtn Cartridges can make brass for you as they did for me.  Cody cuts the case from solid rod stock.  The cases are very solid.  I suggest you anneal before shooting and on the first shot use a fixed bullet with crimp.  You need to fire form the brass to seal the chamber if you plan to breech load for best accuracy.   